NanoClear Test Pen
Harmonization Code : 3405.90.90.00 | Polishes and creams, for footwear, furniture, floors, coachwork, glass or metal, scouring pastes and powders and similar preparations; Other; Other
Main features
- Best-in-class stencil treatment technology
- Simple and effective test
- No training required
Product Description
Aculon® NanoClear® Test Pen technology enables a simple and effective test for the proper application of Aculon's NanoClear Fluxophobic Stencil Treatment Wipes.
Benefits of Aculon's NanoClear® Test Pen
- Confirm effective application & continued presence of Aculon® NanoClear® Stencil Treatment
- Fast and effective results
- No capital equipment investment required
- Easy to apply
Note: It is only possible to order a test pen in combination with an order of Nanoclear® Wipes. For each purchase of 20 wipes, it is possible to order a test pen.
TDS, SDS & Technical Documents
Technical Specifications
No specifications available.
Additional Information
How to apply the Nanoclear Test Pen
|
STEP 1 ⇨ CLEAN |
STEP 2 ⇨ TEST |
STEP 3 ⇨ INTERPRET RESULTS |
|
The surface must not be contaminated prior to testing. |
To use the pen, place the stencil on a clean, level surface. Ensure the stencil is at room temperature. Then, draw the test pen across the stencil surface to be tested. Make three passes and evaluate the third pass only. |
PASS - If the third ink swath beads up, tears apart, or shrinks into a thin line then this surface has the Aculon NanoClear® fluxophobic coating on the surface. FAIL - If the third ink swath remains wetted (outline appears) on the test sample for three seconds or more then this surface does not have the Aculon NanoClear® fluxophobic coating on the surface. Apply NanoClear Fluxophobic stencil treatment.
|
Application Tips
- Discard contaminated test pens.
- Use a “Fresh” test pen. NanoClear Test pens are good for 6 months from the production date.
- Never re-test the same location. Move along the sample or test a new area.
- Clean the test area with IPA or DI water and a clean room wipe prior to using the stencil.